N° 629
|
Отличие лицевой стороны бумажного полотна от оборотной стороны Необходимо отличить оборотную сторону желтого, а также белого бумажного полотна от лицевой стороны соответствующего бумажного полотна.
Front side – backside differentiation of paper web
The backside of yellow and white paper web should be differentiated from the respective front side.
|
|
N° 549
|
Gloss measurement of transparent plastic films
The gloss factor of different transparent plastic films should be measured on both sides.
|
|
N° 521
|
Gloss measurement of anodized guide rails
The gloss of anodized aluminum guide rails should be inline measured.
|
|
N° 510
|
Gloss measurement of translucent plastic films
The gloss level of semi-transparent plastic films should be inline measured.
|
|
N° 495
|
Gloss measurement on coated textiles
The gloss of fabrics will be influenced from a special coating and the task should be an inline measurement of the gloss value.
|
|
N° 489
|
Gloss measurement on polished slabs
The gloss of polished slabs should be measured.
|
|
N° 246
|
Gloss measurement of the primer surface on a vane
The gloss factor of the primer surface of vanes from wind turbines should be measured contactless. At this, the gloss sensor is mounted on a robot and will be moved vertically to make sure, that the distance to the primer surface of the vane remains approximately at 15mm, simultaneously the vane will be moved horizontally so that the gloss factor can be measured along the long axis of the vane. Normally the gloss factor of the primer surface should be lower than 5 in order to guarantee that the following coating get a fix compounding to the primer surface.
|
|
N° 185
|
Gloss measurement of the glass surface of a photo voltaic panel
The gloss factor of the glass cover of a photo voltaic panel should be measured during the production.
|
|
N° 183
|
Differentiation of front side and back side from a sound damping carpet
The front side should be distinguished from the back side of a sound damping carpet.
|
|
N° 151
|
Differentiation of leather imitations
Two black leather imitations should be differentiated and the gloss factor should be documented with a gloss measurement device.
|
|
N° 100
|
Gloss inline measurement after the varnish of doors
Immediately after the varnish of the doors the gloss factor should be controlled. Tests have shown that the amount of varnish, which will be sprayed onto the door surface, influences the gloss factor. If not enough varnish is used the surface becomes rough.
|
|
N° 87
|
Inline gloss measurement on abrasive belts
The gloss factor is a significant parameter for the surface quality, the roughness, of an abrasive belt. Thus a gloss measurement inline sensor should be used for quality control of the abrasive surface.
|
|
N° 74
|
Inline gloss measurement of plastic films and laminated plates
During the production of plastic films as well as of laminated plates the gloss factor should be measured.
|
|
N° 67
|
Inline gloss control in the furniture industry
During the manufacturing process of doors just after the painting line the amount of color must be controlled.
|
|
N° 16
|
Detection of glossy regions on a matt-finished glass plate
During the production of matt-finished glass plates the matt-finished surface must be controlled particularly with regard to small glossy spot. The glossy domains which should be detected are starting with a diameter of approximately 3 mm.
|
|